Here is our chamber. It is made w/ .2mm We make as much as possible out of polycarb and/or acrylic so that we can solvent weld it. The wire ports were sealed w/aquarium silicone. We also used it on t… (View Post)
We have been using .2mm wire to save cost. The anode dissolves within a week of electrophoresis. Has anyone noticed loss material on the anode with .5mm wire? FYI, We also built a chamber with stainl… (View Post)